Endoscopy before the work, the in-place cleaning process and endoscopy after cleaning of spiral-wound water-cooled oil bath coolers of pump units.
Input data: AISI 316L; tube 12×1 mm, length 22 m; rated pressure 3 bar. Before cleaning — hard deposits 1.5–2.5 mm thick narrowing the tube bore. After CPR the heat transfer surface is clean and insoluble particles are removed.
CPR Technology — Cleaning Heat Exchangers to Bare Metal
High-Pressure Cleaning vs. CPR Technology: Residual Deposits vs. Bare Metal
Spiral-Wound Gas Cooler — Endoscopy After CPR Cleaning
Spiral-Wound Pump Bearing Oil Cooler — CPR Cleaning
Gas Cycle Cooler OGTs (OK 700-1) — CPR Cleaning
ChME3 Locomotive Fuel Heater — CPR Cleaning Video Report